Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 102 °C | 216 °F | ISO 306 |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Vicat Softening Point | 102 °C | 216 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Vicat Softening Point | 102 °C | 216 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 82 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 102 °C | 216 °F | 50°C/h 10N; ISO 306 |
DSM Yparex® 8102 E Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Vicat Softening Point | 102 °C | 216 °F | Rate B; ASTM D1525 |
Ineos Nova FX510 Super High Impact Polystyrene
(discontinued **) Features: Extremely high impact strengthGood flexural strengthUL Classification 94 HBCustom colors availableApplications: Injection molding or extrusionSuitable replacement for some engineering resi.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
Ineos Nova 2590 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistance, USP Class VIApplications: Consumer electronics, Housewares, Co-extrusion cap coat, Impact resin cuttingExposure to gamma radi.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
Ineos Nova 5810 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |
|||
Vicat Softening Point | 102 °C | 216 °F | 50°C/h 10N; ISO 306 |
Yparex 8102 Polyolefin Adhesive Resin The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Vicat Softening Point | 102 °C | 216 °F | VST/B/50; ISO 306 |
GEHR Plastics PMMA Acrylic Polymethylmethacrylate is refractory and shows a good mechanical strength, tensile strength and hardness. PMMA is also scratch resistant and easy to polish. It shows good temperature resistance and .. |
|||
Vicat Softening Point | 102 °C | 216 °F | |
Ineos Styrenics Polystyrene 147F (NAFTA) An easy flow, general purpose polystyrene. Has moderate heat resistance and strength for general molding and extrusion applications.Information provided by BASF.Ineos Styrenics purchased this produ.. |
|||
Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ISO 306B |
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ISO 306A |
Lucite International Elvakon® 4470 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ISO 306B |
Lucite International Elvakon® 4474 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Vicat Softening Point | 102 °C | 216 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SP 255 Toughened Polystyrene Characteristics Superior flexibility Excellent flow grade High ball drop strength Good clarityProcessing Extrusion Thermoforming Injection MoldingApplications Transparent hangers, stationery it.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Vicat Softening Point | 102 °C | 216 °F | A (10N); ISO 306 |
Borealis Himod™ FT7294 LDPE for Film Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Vicat Softening Point | 102 °C | 216 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSC 1450N High Heat Resistance Polystyrene 1450N is a high heat resistance, easy flowing crystal polystyrene for the production of thick insulation board. The low viscosity of this grade makes it particularly suitable for the production of .. |
|||
Vicat Softening Point | 102 °C | 216 °F | 120°C/hr, 9.8N; ASTM D1525 |
Lubrizol Estane® 2103-90AEL Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Vicat Softening Point | 102 °C | 215 °F | ASTM D1525 |
Chevron Phillips EB6755 Rubber Modified Polystyrene DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practi.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
Chevron Phillips Marlex® 4538A LDPE Blow Molding Resin Resin Type: HomopolymerCharacteristics: High Melt Strength, Good Parison Control, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on Gloss, Long Standing .. |
|||
Vicat Softening Point | 102 °C @Load 1.00 kg, Thickness 3.17 mm |
216 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers Diamaloy ABS VP-22 Flame Retardant ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 102 °C | 216 °F | 50°C/hr; ASTM D1525 |
Chi Mei Acryrex® CM-211 PMMA Features:Good Weather ResistanceHigh ClarityHigh FlowHigh GlossHigh Heat ResistanceHigh ViscosityUses:ContainersCosmeticsHousehold GoodsKnobsRoHS CompliantAppearance: Clear/TransparentForms: Pellets.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
Americas Styrenics STYRON® 478 High Impact Polystyrene Product CharacteristicsGood glossExcellent balance of flow and stiffnessFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsIn.. |
|||
Vicat Softening Point | 102 °C | 216 °F | ASTM D1525 |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Vicat Softening Point | 102 °C @Load 5.00 kg |
216 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |