Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 101 °C | 214 °F | B |
Plastcom SLOVALEN PH 99 GB 30 LS PP, 30% glass beads, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Vicat Softening Point | 101 °C | 214 °F | ASTM D1525 |
SABIC 6821N Linear Low Density Polyethylene for Blown Film Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi.. |
|||
Vicat Softening Point | 101 °C @Load 1.00 kg |
214 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 U represents the version of Flexirene FG 20 U.. |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® INP564 ABS SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® MG34LG ABS Automotive: Low gloss ABS for unpainted interior applications. |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycolac® MG37CR ABS (Asia Pacific) High performance, injection molding ABS. Overall balance of physical properties, good processability and chemical resistance.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 101 °C | 213 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Vicat Softening Point | 101 °C | 214 °F | |
Americas Styrenics Styron® 615APR Polystyrene
(discontinued **) STYRON® 615 APR is a general purpose easy flow resin typically used for medical, pharmaceutical and thin-walled parts. It is an excellent resin for blending with K-Resin (K-Resin is a trademark of .. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Vicat Softening Point | 101 °C | 214 °F | ASTM D1525 |
Ineos Nova 731G High Impact Polystyrene
(discontinued **) Balance of stiffness and toughness, High impact, USP Class VIApplications: Razor components, Personal care, Consumer goodsIn addition, exposure to gamma radiation in the 2.02-6.06 megarad range ahs .. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 1000 g; ASTM D1525 |
LG Chemical MI-770 MIPS |
|||
Vicat Softening Point | 101 °C | 214 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |
|||
Vicat Softening Point | 101 °C | 214 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 101 °C @Load 1.02 kg |
213 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 3100/3101 GPPS Good balance of flow and set-up propertiesModerate heat resistanceUSP Class VI certifiedInformation provided by Styrolution |
|||
Vicat Softening Point | 101 °C @Load 1.02 kg |
214 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 5300 HIPS Excellent ESCRFree of zinc additivesMatte, easily decorated finishGood toughnessUL Classification 94 HBInformation provided by Styrolution |
|||
Vicat Softening Point | 101 °C | 214 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 101 °C | 214 °F | ISO R-306 |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 101 °C | 214 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SP 265 Toughened Polystyrene CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Ther.. |
|||
Vicat Softening Point | 101 °C | 214 °F | ASTM D1525 |
Lubrizol Isoplast® 2530 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSC 1960N Crystal Polystyrene 1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® FR 3008 HR Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeHDT/A = 85 °CVicat/B 120 temperature = 103 °CUL-listing 94 V-0 (1.5 mm)improved chemical and very good hydrolysis resistance antimony-, chlorine- and bromine-free flame.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® FR 3020 Polycarbonate + ABS, Mineral Filled 5 % mineral filledfor thin-wall applicationsinjection moldingVicat/B 120 = 103 °CHDT/A = 85 °Cvery good UL listing in small wall thickness (V-0 at 0.75 mm)PreprocessingMax. Water content |
|||
Vicat Softening Point | 101 °C | 214 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/hr; 50N |
Arkema Group Oroglas® V 920 T Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 T is an injection molding grade with an improved thermal resistance HDT A ( 1.82 MPa ) = 96°c without any adverse effect on mechanical and optical properties.The processing of OROGLAS.. |
|||
Vicat Softening Point | 101 °C | 214 °F | 50°C/h 50N |
Ineos ABS Centrex® HGM ASA Blend
(discontinued **) Key Features:UnfilledLight stabilized or stable to lightU.V. stabilized or stable to weatherHeat stabilized or stable to heatSuitable processing methods:Injection moldingInformation provided by Baye.. |