Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 100 °C | 212 °F | B |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® MG94 ABS (Europe-Africa-Middle East) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific) CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa.. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Vicat Softening Point | 100 °C | 212 °F | |
Polycasa Acryl® G 77 E Acrylic, Extrusion Grade Extrusion grade for semi-finished products such as profile, sheet and tubes; TV-, HiFi - and video-windows.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Network Polymers 351 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525/A |
Gichem GILAC A50VX35/VO ABS Flame Retardant
(discontinued **) ABS self-extinguishing class V0, 17% glass fiber filled, good stiffness. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
LyondellBasell Plexar® PX3060 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and .. |
|||
Vicat Softening Point | 100 °C | 212 °F | 1 kg; ASTM D1525 |
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding High flowability gradeParticularly recommended for complicated profiles or large and thin wall partsFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface har.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Mitsui ADMER® NF458A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Vicat Softening Point | 100 °C | 212 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin Polycarbonate-resin-based halogen-free flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even a.. |
|||
Vicat Softening Point | 100 °C | 212 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 100 °C @Temperature 50.0 °C |
212 °F @Temperature 122 °F |
ISO 306 |
Styrolution Terluran® HD-15 ABS Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 100 °C | 212 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati.. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl HF180 PPE+HIPS (Europe-Africa-Middle East) NORYL HF180 is an unfilled, flame retardant material with a Vicat B/120 of 100°C according ISO 306. NORYL HF180 is V1 at 2.0 mm according UL94 and halogenThis data was supplied by SABIC-IP for th.. |
|||
Vicat Softening Point | 100 °C @Load 5.10 kg |
212 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution Novodur® 240 ABS Novodur 240 is an injection molding grade of ABS with standard impact strength and high gloss.Information provided by Styrolution |
|||
Vicat Softening Point | 100 °C | 212 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate Plasticizer 33%. Weight loss on heating = 3.6% per ASTM D 707. Soluble matter loss = 0.6% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 100 °C | 212 °F | JIS-K-6740 |
Denka VINYKON M1071 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Ashley Polymers Ashlene® ABS R214 Reprocessed for general purpose, general application, requiring good impact properties.Data provided by the manufacturer |
|||
Vicat Softening Point | 100 °C | 212 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 100 °C @Load 5.00 kg |
212 °F @Load 11.0 lb |
|
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM-D1525 |
Polyram BondyRam® 4001 Maleic Anhydride modified LLDPE coupling agent
(discontinued **) Maleic Anhydride grafted linear low density polyethylene recommended as a coupling agent in PE composites with minerals and wood and compatibilizer in PE/PA blendsInformation provided by Polyram Ram.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |