Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 67.0 GPa @Temperature 677 °C |
9720 ksi @Temperature 1250 °F |
|
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Shear Modulus | 67.0 GPa @Temperature 677 °C |
9720 ksi @Temperature 1250 °F |
|
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F) Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Shear Modulus | 67.0 GPa @Temperature 677 °C |
9720 ksi @Temperature 1250 °F |
|
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Shear Modulus | 67.0 GPa @Temperature 93.0 °C |
9720 ksi @Temperature 199 °F |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |
|||
Shear Modulus | 67.0 GPa @Temperature 700 °C |
9720 ksi @Temperature 1290 °F |
|
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |
|||
Shear Modulus | 67.0 GPa @Temperature 677 °C |
9720 ksi @Temperature 1250 °F |
|
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include .. |
|||
Shear Modulus | 67.0 GPa @Temperature 316 °C |
9720 ksi @Temperature 601 °F |
|
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-.. |