Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.93 GPa @Temperature -30.0 °C |
280 ksi @Temperature -22.0 °F |
DAM; ISO 6721 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Shear Modulus | 1.93 GPa @Temperature -50.0 °C |
280 ksi @Temperature -58.0 °F |
DAM; ISO 6721 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |