Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.00 GPa @Temperature 70.0 °C |
145 ksi @Temperature 158 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Shear Modulus | 1.00 GPa @Temperature 20.0 °C |
145 ksi @Temperature 68.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Shear Modulus | 1.00 GPa @Temperature 200 °C |
145 ksi @Temperature 392 °F |
|
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason E 6020 P PES Ultrason E 6020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes of high molecular weight and good solubility in typical solvents (N-Methylpyrrolidone, Dimethylacetamide, Dichl.. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Shear Modulus | 1.00 GPa @Temperature 50.0 °C |
145 ksi @Temperature 122 °F |
ISO 6721 |
BASF Ultrason E 2020 P PES Ultrason E 2020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes, for solvent based processes; product is soluble e.g. in N-Methylpyrrolidone and N,N-Dimethylacetamide. |