Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Modulus = 67.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 67.0 GPa

@Temperature 677 °C
9720 ksi

@Temperature 1250 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 67.0 GPa

@Temperature 677 °C
9720 ksi

@Temperature 1250 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 67.0 GPa

@Temperature 677 °C
9720 ksi

@Temperature 1250 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Shear Modulus 67.0 GPa

@Temperature 93.0 °C
9720 ksi

@Temperature 199 °F
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy
The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt..
Shear Modulus 67.0 GPa

@Temperature 700 °C
9720 ksi

@Temperature 1290 °F
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy
INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor..
Shear Modulus 67.0 GPa

@Temperature 677 °C
9720 ksi

@Temperature 1250 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include ..
Shear Modulus 67.0 GPa

@Temperature 316 °C
9720 ksi

@Temperature 601 °F
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel
INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-..