Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 65.0 MPa @Temperature -54.0 °C |
9430 psi @Temperature -65.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Shear Strength | 65.0 MPa @Temperature 232 °C |
9430 psi @Temperature 450 °F |
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64% |
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel |