Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.41 MPa @Temperature 149 °C |
930 psi @Temperature 300 °F |
Double Lap Shear (Composite/Composite), 0.05 psf, No conditioning |
Hexcel® Redux® 330K Epoxy film adhesives for the bonding and finishing of composites Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl.. |
|||
Shear Strength | 6.41 MPa @Temperature 149 °C |
930 psi @Temperature 300 °F |
Double Lap Shear (Composite/Composite), 0.03 psf, No conditioning |
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl.. |
|||
Shear Strength | 6.41 MPa @Temperature 23.0 °C |
930 psi @Temperature 73.4 °F |
Overlap, ABS |
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 6.41 MPa @Temperature 23.0 °C |
930 psi @Temperature 73.4 °F |
Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |