Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 60.7 MPa @Temperature 150 °C |
8800 psi @Temperature 302 °F |
ASTM D732 |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest.. |
|||
Shear Strength | 60.7 MPa @Temperature 150 °C |
8800 psi @Temperature 302 °F |
ASTM D732 |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI) Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda.. |
|||
Shear Strength | 60.7 MPa @Temperature 82.2 °C |
8800 psi @Temperature 180 °F |
0° Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |
|||
Shear Strength | 60.7 MPa @Temperature 23.0 °C |
8800 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel |
|||
Shear Strength | 60.7 MPa @Temperature 23.0 °C |
8800 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel |