Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 48.0 MPa @Temperature 132 °C |
6960 psi @Temperature 270 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel |