Mechanical Properties Metric English Comments
Shear Strength 44.8 MPa

@Temperature 23.9 °C
6500 psi

@Temperature 75.0 °F
Short-Beam, Dry, Autoclave with Post-Cure; ASTM D2344
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Shear Strength 44.8 MPa

@Temperature 21.1 °C
6500 psi

@Temperature 70.0 °F
Short-Beam, Wet; ASTM D2344
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Shear Strength 44.8 MPa

@Temperature 71.1 °C
6500 psi

@Temperature 160 °F
Short-Beam, Dry; ASTM D2344
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Shear Strength 44.8 MPa

@Temperature 177 °C
6500 psi

@Temperature 351 °F
Short Beam
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric
Information provided by HexCel