Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 37.9 MPa @Temperature 87.8 °C |
5500 psi @Temperature 190 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Shear Strength | 37.9 MPa @Temperature 71.1 °C |
5500 psi @Temperature 160 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Shear Strength | 37.9 MPa @Temperature 210 °C |
5500 psi @Temperature 410 °F |
Inter-laminar, Wet; SACMA SRM 7R-94 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Shear Strength | 37.9 MPa @Temperature 232 °C |
5500 psi @Temperature 450 °F |
T300, Plain Weave; Fill Short Beam; AMC |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Fabric Form Fiber: T300-3KInformation provided by HexCel |
|||
Shear Strength | 37.9 MPa @Temperature 71.1 °C |
5500 psi @Temperature 160 °F |
Lap Shear |
Hexcel® Redux® 312L Modified epoxy film adhesive Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Shear Strength | 37.9 MPa @Temperature 24.0 °C |
5500 psi @Temperature 75.2 °F |
Overlap |
3M Scotch-Weld™ 1386 One-Part Epoxy Adhesives and Metal Primer High Temperature strength and Impact resistanceInformation provided by 3M |