Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.70 MPa @Temperature 22.2 °C |
536 psi @Temperature 72.0 °F |
Aluminum Double Lap Shear (0.06 inch gap) |
Hexcel® Redux® 206-NA Foaming adhesive film The Redux 200 series is a range fo foaming adhesive films presented in sheet form. They expand during the cure cycle to fill gaps and adhere strongly to all parts of the structure with which they co.. |
|||
Shear Strength | 3.70 MPa @Temperature 75.0 °C, Time 1.81e+6 sec |
536 psi @Temperature 167 °F, Time 504 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Shear Strength | 3.70 MPa @Temperature 75.0 °C, Time 1.81e+6 sec |
536 psi @Temperature 167 °F, Time 504 hour |
Overlap, 1/8" Birch/Birch |
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |