Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 23.7 MPa @Temperature 23.9 °C |
3440 psi @Temperature 75.0 °F |
Arovex (abraded), with Arovex Carbon Fiber Epoxy Laminate |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods.. |
|||
Shear Strength | 23.7 MPa @Temperature 23.9 °C |
3440 psi @Temperature 75.0 °F |
Arovex (abraded), with Arovex Carbon Fiber Epoxy Laminate |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Paste Epovex® Adhesive Paste is a carbon nanotube enhanced two part epoxy adhesive thixotropic paste. Used for bonding or filling, Epovex Paste is ideal for many metals, woods, masonry products, and some.. |