Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 22.99 MPa @Temperature 149 °C |
3335 psi @Temperature 300 °F |
Lap Shear Unprimed, No conditioning of Redux 319 |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 22.99 MPa @Temperature 149 °C |
3335 psi @Temperature 300 °F |
Lap Shear Primed, No conditioning of Redux 319 |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 22.99 MPa @Temperature 149 °C |
3335 psi @Temperature 300 °F |
Lap Shear |
Hexcel® Redux® 322 Modified epoxy film adhesive (0.078 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |