Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.234 MPa @Shear Rate 5000 1/s, Temperature 280 °C |
33.9 psi @Shear Rate 5000 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**) 33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Shear Strength | 0.234 MPa @Shear Rate 500 1/s, Temperature 220 °C |
33.9 psi @Shear Rate 500 1/s, Temperature 428 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |