Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 22.0 MPa @Temperature 149 °C |
3190 psi @Temperature 300 °F |
Lap Shear |
Hexcel® Redux® 319L High Performance Modified Epoxy Film Adhesive (0.036 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 22.0 MPa @Temperature 21.1 °C |
3190 psi @Temperature 70.0 °F |
Lap Shear |
Hexcel® Redux® 322 Modified epoxy film adhesive (0.06 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |
|||
Shear Strength | 22.0 MPa @Temperature 21.1 °C |
3190 psi @Temperature 70.0 °F |
Lap Shear |
Hexcel® Redux® 322 Modified epoxy film adhesive (0.078 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |
|||
Shear Strength | 22.0 MPa @Temperature 21.1 °C |
3190 psi @Temperature 70.0 °F |
Lap Shear |
Hexcel® Redux® 322U Modified epoxy film adhesive (0.06 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |
|||
Shear Strength | 22.0 MPa @Temperature 120 °C |
3190 psi @Temperature 248 °F |
Lap Shear; Cured 5 days at 23°C; Substrate: 2024 T3 Aluminum Alloy (CSA pretreated, Unprimed); EN2243-1 |
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive Redux 870 A/B is a two component high performance epoxy paste adhesive, ideal for use as a Liquid Shim or for potting applications. This high temperature performing thixotropic adhesive has been spe.. |