Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.207 MPa @Temperature 22.2 °C |
30.0 psi @Temperature 72.0 °F |
Lap Shear Unprimed, 12 months at 300°F |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 0.207 MPa @Temperature 107 °C |
30.0 psi @Temperature 225 °F |
Overlap, 1/8 birch to 1/8 birch, bond tested after aging 3 weeks @ 24°C and 50% RH at a separation rate of 0.2 in/min; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 0.207 MPa @Temperature 93.0 °C |
30.0 psi @Temperature 199 °F |
Overlap, 1/8" birch 1/8" birch |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Shear Strength | 0.207 MPa @Temperature 82.0 °C |
30.0 psi @Temperature 180 °F |
1/8" Birch/High-Pressure Laminate, no aging |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Shear Strength | 0.207 MPa @Temperature 150 °C |
30.0 psi @Temperature 302 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9082 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.207 MPa @Temperature 150 °C |
30.0 psi @Temperature 302 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9082UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.207 MPa @Temperature 107 °C |
30.0 psi @Temperature 225 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.207 MPa @Temperature 107 °C |
30.0 psi @Temperature 225 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.207 MPa @Temperature 93.0 °C |
30.0 psi @Temperature 199 °F |
Overlap, 1/8" birch 1/8" birch |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Shear Strength | 0.207 MPa @Temperature 82.0 °C |
30.0 psi @Temperature 180 °F |
1/8" Birch/High-Pressure Laminate, no aging |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |