Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 9.31 MPa @Temperature 204 °C |
1350 psi @Temperature 400 °F |
ASTM D732 |
Greene Tweed Avalon® 56 PTFE PTFE is used in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use.. |
|||
Shear Strength | 9.31 MPa @Temperature 23.0 °C |
1350 psi @Temperature 73.4 °F |
Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ TE031 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |