Mechanical Properties Metric English Comments
Shear Strength 90.3 MPa

@Temperature 104 °C
13100 psi

@Temperature 220 °F
+/- 45° In-Plane, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber
Information provided by HexCel