Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 73.8 MPa @Temperature 82.2 °C |
10700 psi @Temperature 180 °F |
Beam, V-Notched; Wet; Vacuum/Oven Cured; ASTM D5379-93 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 74.0 MPa @Temperature 24.0 °C |
10700 psi @Temperature 75.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel |