Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 71.7 MPa @Temperature 21.1 °C |
10400 psi @Temperature 70.0 °F |
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 71.7 MPa @Temperature 82.2 °C |
10400 psi @Temperature 180 °F |
Beam, V-Notched; Wet; Autoclave Cured; ASTM D5379-93 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 71.7 MPa @Temperature 71.1 °C |
10400 psi @Temperature 160 °F |
0° Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 71.7 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Shear Strength | 72.0 MPa @Temperature 24.0 °C |
10400 psi @Temperature 75.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Shear Strength | 72.0 MPa @Temperature 132 °C |
10400 psi @Temperature 270 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel |
|||
Shear Strength | 72.0 MPa @Temperature -54.0 °C |
10400 psi @Temperature -65.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Shear Strength | 71.7 MPa @Temperature 71.0 °C |
10400 psi @Temperature 160 °F |
Short Beam, 1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, T5A120 Carbon Tape Hexcel designation: TXX120-12"-F515; Fiber: IM6Information provided by HexCel |
|||
Shear Strength | 71.7 MPa @Temperature 232 °C |
10400 psi @Temperature 450 °F |
Short Beam; 424 Hrs |
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 72.0 MPa @Temperature 177 °C |
10400 psi @Temperature 351 °F |
IM7 (12K); [+/- 45°]2s; In Plane; Wet condition |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form Fiber: IM7-12KInformation provided by HexCel |
|||
Shear Strength | 71.7 MPa @Temperature 177 °C |
10400 psi @Temperature 351 °F |
Autoclave Cured; [+/- 45°]2s |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |