Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.0689 MPa @Temperature 230 °C |
10.0 psi @Temperature 446 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.0689 MPa @Temperature 230 °C |
10.0 psi @Temperature 446 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.0689 MPa @Time 86400 sec |
10.0 psi @Time 24.0 hour |
Overlap |
3M Weatherban™ 5354 Sealant Tape 3M™ Weatherban™ Sealant Tape 5354 is a high tack extruded synthetic rubber, non-curing sealant in tape form.It can be used to seal between glass, metal, wood and many plastics.Easy to compress and.. |
|||
Shear Strength | 0.0689 MPa @Time 86400 sec |
10.0 psi @Time 24.0 hour |
Overlap |
3M Weatherban™ 5354 Sealant Tape 3M™ Weatherban™ Sealant Tape 5354 is a high tack extruded synthetic rubber, non-curing sealant in tape form.It can be used to seal between glass, metal, wood and many plastics.Easy to compress and.. |