Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 82.0 MPa @Temperature 82.2 °C |
11900 psi @Temperature 180 °F |
Beam, V-Notched; Dry; Vacuum/Oven Cured; ASTM D5379-93 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 82.0 MPa @Temperature 149 °C |
11900 psi @Temperature 300 °F |
Short Beam; Dry; ASTM D2344 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Shear Strength | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, T5A120 Carbon Tape Hexcel designation: TXX120-12"-F515; Fiber: IM6Information provided by HexCel |
|||
Shear Strength | 82.0 MPa @Temperature 24.0 °C |
11900 psi @Temperature 75.2 °F |
Short Beam, Dry |
Hexcel® HexPly® F522 Epoxy Resin, T2C145 Carbon Tape Hexcel designation: T_145-12"-F522; Various Fibers; (145 g/m2)Information provided by HexCel |
|||
Shear Strength | 82.0 MPa @Temperature 232 °C |
11900 psi @Temperature 450 °F |
IM7 (12K); [+/- 45°]2s; In Plane |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form Fiber: IM7-12KInformation provided by HexCel |