Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 72.0 MPa @Temperature 24.0 °C |
10400 psi @Temperature 75.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Shear Strength | 72.0 MPa @Temperature 132 °C |
10400 psi @Temperature 270 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel |
|||
Shear Strength | 72.0 MPa @Temperature -54.0 °C |
10400 psi @Temperature -65.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel |
|||
Shear Strength | 72.0 MPa @Temperature 177 °C |
10400 psi @Temperature 351 °F |
IM7 (12K); [+/- 45°]2s; In Plane; Wet condition |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form Fiber: IM7-12KInformation provided by HexCel |