Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 5.00 MPa @Temperature -55.0 °C |
725 psi @Temperature -67.0 °F |
Beam Shear, No conditioning |
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl.. |
|||
Shear Strength | 5.00 MPa @Temperature 21.1 °C |
725 psi @Temperature 70.0 °F |
Beam Shear, No conditioning |
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl.. |
|||
Shear Strength | 5.00 MPa @Temperature 71.1 °C |
725 psi @Temperature 160 °F |
Beam Shear, No conditioning |
Hexcel® Redux® 330M Epoxy film adhesives for the bonding and finishing of composites Redux 330 is a 350°F curing tough film adhesive which is ideally suited to structural bonding, composite to composite bonding, surface finishing, electromagnetic shielding and lightning strike appl.. |