Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 44.8 MPa @Temperature 23.9 °C |
6500 psi @Temperature 75.0 °F |
Short-Beam, Dry, Autoclave with Post-Cure; ASTM D2344 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Shear Strength | 44.8 MPa @Temperature 21.1 °C |
6500 psi @Temperature 70.0 °F |
Short-Beam, Wet; ASTM D2344 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Shear Strength | 44.8 MPa @Temperature 71.1 °C |
6500 psi @Temperature 160 °F |
Short-Beam, Dry; ASTM D2344 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Shear Strength | 44.8 MPa @Temperature 177 °C |
6500 psi @Temperature 351 °F |
Short Beam |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |