Polymer Property : Shear Strength = 25.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 25.4 MPa

@Temperature 23.9 °C
3690 psi

@Temperature 75.0 °F
(+7 days water soak), with Arovex Carbon Fiber Epoxy Laminate
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid
Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods..
Shear Strength 25.4 MPa

@Temperature 25.0 °C
3690 psi

@Temperature 77.0 °F
Tensile, Al/Al lap joint; cured 2 hours @ 93°C
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy
This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic..