Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 19.9 MPa @Temperature 23.9 °C |
2880 psi @Temperature 75.0 °F |
Cure cycle: 7 days @ RT (+7 days ethyl alcohol soak), with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods.. |