Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.552 MPa @Temperature 82.0 °C |
80.0 psi @Temperature 180 °F |
1/8" Birch/High-Pressure Laminate, aged 3 mo |
3M Fastbond™ 30-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |
|||
Shear Strength | 0.552 MPa @Temperature 23.0 °C |
80.0 psi @Temperature 73.4 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.552 MPa @Temperature 23.0 °C |
80.0 psi @Temperature 73.4 °F |
Over-Lap Shear on Stainless Steel; ASTM D1002 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Shear Strength | 0.552 MPa @Temperature 82.0 °C |
80.0 psi @Temperature 180 °F |
1/8" Birch/High-Pressure Laminate, aged 3 mo |
3M Fastbond™ 30H-NF Contact Adhesive 3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M |