Polymer Property : Shear Strength = 0.234 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.234 MPa

@Shear Rate 5000 1/s,
Temperature 280 °C
33.9 psi

@Shear Rate 5000 1/s,
Temperature 536 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
33% Glass Reinforced Polyamide 612 Zytel 77G33L BK031 is a 33% glass fiber reinforced black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Shear Strength 0.234 MPa

@Shear Rate 500 1/s,
Temperature 220 °C
33.9 psi

@Shear Rate 500 1/s,
Temperature 428 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers