Polymer Property : Shear Strength = 0.01727 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.01727 MPa

@Shear Rate 50.0 1/s,
Temperature 300 °C
2.505 psi

@Shear Rate 50.0 1/s,
Temperature 572 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers