Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 60.0 MPa @Temperature 275 °C |
8700 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Flexural Strength | 60.0 MPa @Temperature 275 °C |
8700 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Flexural Strength | 60.0 MPa @Temperature 275 °C |
8700 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Flexural Strength | 60.0 MPa @Temperature 80.0 °C |
8700 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 60.0 MPa @Treatment Temp. 200 °C, Time 3600 sec |
8700 psi @Treatment Temp. 392 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica.. |
|||
Flexural Strength | 60.0 MPa @Thickness >=200 mm |
8700 psi @Thickness >=7.87 in |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |
|||
Flexural Strength | 60.0 MPa @Temperature 120 °C |
8700 psi @Temperature 248 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |