Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 496 MPa @Temperature 21.1 °C |
72000 psi @Temperature 70.0 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Strength | 496 MPa @Temperature 23.9 °C |
72000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi.. |
|||
Flexural Strength | 496 MPa @Temperature 71.1 °C |
72000 psi @Temperature 160 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s.. |