Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 470 MPa @Treatment Temp. 20.0 °C, Time 3600 sec |
68200 psi @Treatment Temp. 68.0 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Flexural Strength | 470 MPa @Treatment Temp. 100 °C, Time 3600 sec |
68200 psi @Treatment Temp. 212 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |