Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 296 MPa @Temperature 87.8 °C |
43000 psi @Temperature 190 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |