Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 284 MPa @Temperature 23.0 °C |
41200 psi @Temperature 73.4 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |