Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 185 MPa @Temperature 175 °C |
26800 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
Flexural Strength | 185 MPa @Strain 6.00 % |
26800 psi @Strain 6.00 % |
Conditioned; ISO 178 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Strength | 185 MPa @Strain 5.00 % |
26800 psi @Strain 5.00 % |
ISO 178 |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Flexural Strength | 185 MPa @Strain 5.00 % |
26800 psi @Strain 5.00 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 185 MPa @Temperature 80.0 °C |
26800 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 185 MPa @Temperature -40.0 °C |
26800 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 185 MPa @Temperature 23.0 °C |
26800 psi @Temperature 73.4 °F |
Result based on HT G22; ISO 178 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |