Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 165 MPa @Thickness 1.57 mm |
24000 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |