Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 70.0 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
Flexural Strength | 70.0 MPa @Temperature 275 °C |
10200 psi @Temperature 527 °F |
ISO 178 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Flexural Strength | 70.0 MPa @Temperature 275 °C |
10200 psi @Temperature 527 °F |
ISO 178 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Flexural Strength | 70.0 MPa @Strain 6.00 % |
10200 psi @Strain 6.00 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 70.0 MPa @Temperature 80.0 °C |
10200 psi @Temperature 176 °F |
Practical Use (Water Absorption 2.5%); ASTM-D790 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 70.0 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 70.0 MPa @Treatment Temp. 250 °C, Time 3600 sec |
10200 psi @Treatment Temp. 482 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Flexural Strength | 70.0 MPa @Treatment Temp. 200 °C, Time 3600 sec |
10200 psi @Treatment Temp. 392 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Flexural Strength | 70.0 MPa @Treatment Temp. 220 °C, Time 3.60e+6 sec |
10200 psi @Treatment Temp. 428 °F, Time 1000 hour |
Four point |
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand .. |