Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 586 MPa @Temperature 23.9 °C |
85000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Flexural Strength | 586 MPa @Temperature 23.9 °C |
85000 psi @Temperature 75.0 °F |
Dry, Autoclave with Post-Cure; ASTM D790 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Flexural Strength | 586 MPa @Temperature 23.9 °C |
85000 psi @Temperature 75.0 °F |
Wet (2 hour water boil); ASTM D790 |
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s.. |
|||
Flexural Strength | 586 MPa @Temperature 82.2 °C |
85000 psi @Temperature 180 °F |
0° Direction, Wet; ASTM D790 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Flexural Strength | 586 MPa @Thickness 1.57 mm |
85000 psi @Thickness 0.0620 in |
LW; ASTM D790 |
Industrial Laminates/Norplex NP130HF Glass Fabric Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens.. |