Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 552 MPa @Temperature 21.1 °C |
80000 psi @Temperature 70.0 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Strength | 552 MPa @Thickness 1.57 mm |
80000 psi @Thickness 0.0620 in |
LW; ASTM D790 |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |