Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 370 MPa @Temperature 23.0 °C |
53700 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Flexural Strength | 370 MPa @Thickness >=100 mm |
53700 psi @Thickness >=3.94 in |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Flexural Strength | 370 MPa @Treatment Temp. 200 °C, Time 3600 sec |
53700 psi @Treatment Temp. 392 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |