Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 280 MPa @Temperature 23.0 °C |
40600 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Flexural Strength | 280 MPa @Temperature 23.0 °C |
40600 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Flexural Strength | 280 MPa @Strain 4.20 % |
40600 psi @Strain 4.20 % |
ISO 178 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Strength | 280 MPa @Temperature 23.0 °C |
40600 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-663G30 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 280 MPa @Temperature 23.0 °C |
40600 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.0%); ASTM-D790 |
Toyobo GLAMIDE® TY-791GT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 280 MPa @Temperature -40.0 °C |
40600 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.4%); ASTM-D790 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 280 MPa @Treatment Temp. 100 °C, Time 3600 sec |
40600 psi @Treatment Temp. 212 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Flexural Strength | 280 MPa @Thickness >=1.50 mm |
40600 psi @Thickness >=0.0591 in |
1hr/150°C/measured at 150°C; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |