Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 275 MPa @Temperature 125 °C |
39900 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 275 MPa @Temperature 125 °C |
39900 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Flexural Strength | 275 MPa @Temperature 23.0 °C |
39900 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Flexural Strength | 275 MPa @Temperature 125 °C |
39900 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Flexural Strength | 275 MPa @Temperature 23.0 °C |
39900 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |