Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 190 MPa @Temperature 125 °C |
27600 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Flexural Strength | 190 MPa @Temperature 125 °C |
27600 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Flexural Strength | 190 MPa @Temperature 125 °C |
27600 psi @Temperature 257 °F |
Result based on 450GL30; ISO 178 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Flexural Strength | 190 MPa @Temperature 175 °C |
27600 psi @Temperature 347 °F |
ISO 178 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Flexural Strength | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Flexural Strength | 190 MPa @Temperature 1000 °C |
27600 psi @Temperature 1830 °F |
|
McDanel Advanced Ceramics MV-HR1 Mullite Mullite (3Al2O3 • 2SiO2) is a refractory oxide material combining low thermal expansion, good mechanical strength, and resilience at elevated temperatures. Mullite is formulated to produce den.. |
|||
Flexural Strength | 190 MPa @Strain 2.70 % |
27600 psi @Strain 2.70 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Strength | 190 MPa @Temperature 23.0 °C |
27600 psi @Temperature 73.4 °F |
Practical Use; ASTM-D790 |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 190 MPa @Treatment Temp. 50.0 °C, Time 3600 sec |
27600 psi @Treatment Temp. 122 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |
|||
Flexural Strength | 190 MPa @Thickness >=100 mm |
27600 psi @Thickness >=3.94 in |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |