Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 149 MPa @Thickness 1.57 mm |
21600 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP680 Paper Base Laminate Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500" |