Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 125 MPa @Temperature 23.0 °C |
18100 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |
|||
Flexural Strength | 125 MPa @Strain 3.50 %, Temperature 23.0 °C |
18100 psi @Strain 3.50 %, Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Flexural Strength | 125 MPa @Strain 7.00 % |
18100 psi @Strain 7.00 % |
Conditioned; ISO 178 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Strength | 125 MPa @Strain 5.80 % |
18100 psi @Strain 5.80 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Flexural Strength | 125 MPa @Temperature 80.0 °C |
18100 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 125 MPa @Temperature -40.0 °C |
18100 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 125 MPa @Temperature -40.0 °C |
18100 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 3.5%); ASTM-D790 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 125 MPa @Temperature -40.0 °C |
18100 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.4%); ASTM-D790 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 125 MPa @Temperature -40.0 °C |
18100 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 3.5%); ASTM-D790 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 125 MPa @Temperature 80.0 °C |
18100 psi @Temperature 176 °F |
Practical Use (Water Absorption 0.8%); ASTM-D790 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 125 MPa @Strain 3.50 %, Temperature 23.0 °C |
18100 psi @Strain 3.50 %, Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Flexural Strength | 125 MPa @Strain 3.50 %, Temperature 23.0 °C |
18100 psi @Strain 3.50 %, Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |