Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 120 MPa @Temperature -40.0 °C |
17400 psi @Temperature -40.0 °F |
ASTM D790 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 120 MPa @Temperature 175 °C |
17400 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 120 MPa @Temperature 175 °C |
17400 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Flexural Strength | 120 MPa @Temperature 275 °C |
17400 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
Flexural Strength | 120 MPa @Temperature 175 °C |
17400 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Flexural Strength | 120 MPa @Temperature 175 °C |
17400 psi @Temperature 347 °F |
ISO 178 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Flexural Strength | 120 MPa @Strain 8.00 % |
17400 psi @Strain 8.00 % |
Conditioned; ISO 178 |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Strength | 120 MPa @Strain 4.80 % |
17400 psi @Strain 4.80 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Strength | 120 MPa @Temperature 80.0 °C |
17400 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 120 MPa @Temperature 23.0 °C |
17400 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 1.7%); ASTM-D790 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 120 MPa @Temperature -40.0 °C |
17400 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 2.5%); ASTM-D790 |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 120 MPa @Temperature 23.0 °C |
17400 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.1%); ASTM-D790 |
Toyobo GLAMIDE® T-663G15 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 120 MPa @Temperature -40.0 °C |
17400 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 3.0%); ASTM-D790 |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 120 MPa @Thickness >=250 mm |
17400 psi @Thickness >=9.84 in |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |